Research Article - (2018) Volume 8, Issue 3

Predicting the Burning Rate of Thermally Thin Nylon Using TGA (Thermo Gravity Analysis) and DSC (Differential Scanning Calorimeter)

Sarat Ganti*
University of Petroleum and Energy Studies, Visakhapatnam, Andhra Pradesh, India
*Corresponding Author: